Tube leakage is commonly caused by corrosion, erosion, vibration, fouling or thermal and mechanical stress. The failure mechanism may originate on either the clean closed-loop side or the open cooling-water side.
Poor water chemistry is one of the main causes. Dissolved oxygen, chlorides, unsuitable pH, depleted corrosion inhibitors and microbial activity can produce pitting or under-deposit corrosion. Seawater and brackish water are especially aggressive, so tube materials must be compatible with their chloride content, temperature and flow velocity.
Excessive water velocity can erode the tube walls, particularly near tube inlets, return bends and areas with disturbed flow. Suspended sand and other solids accelerate this damage. However, very low velocity can also cause problems by allowing sediment and biological deposits to accumulate.
Fouling creates deposits that restrict water flow and cause localized corrosion beneath the deposit layer. Scale also reduces heat transfer, forcing the exchanger to operate at a higher temperature and increasing thermal stress.
Flow-induced vibration can make tubes strike baffles or adjacent tubes, gradually wearing through the wall. Loose or incorrectly spaced baffles, high fluid velocity and two-phase flow can increase vibration risk. Leakage may also develop at expanded or welded tube-to-tube-sheet joints due to poor fabrication, repeated temperature cycling or differential thermal expansion.
Other causes include freezing, water hammer, excessive operating pressure, improper chemical cleaning and galvanic corrosion between dissimilar materials. External chloride contamination during storage can also damage stainless-steel tubes before commissioning.
Leakage can be reduced through correct material selection, controlled water chemistry, suitable flow velocity, effective filtration and regular inspection. Pressure testing, eddy-current testing and analysis of closed-loop water contamination can help locate damaged tubes. Individual leaking tubes may sometimes be plugged temporarily, but widespread deterioration usually requires retubing or tube-bundle replacement.